genus
Clusia
Woods sold under several trade names often come from one genus. These 3 share the genus Clusia, so they are close relatives and frequent substitutes for each other.
0 of 3 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| CupeilloClusia clusioides | 2,210 lbf* | 55.9 lb/ft³ |
| Cupey de monteClusia minor | 509 lbf* | 28.2 lb/ft³ |
| Scotch attorneyClusia rosea | 1,538 lbf* | 47.3 lb/ft³ |