Wood Record

genus

Coccoloba

Woods sold under several trade names often come from one genus. These 5 share the genus Coccoloba, so they are close relatives and frequent substitutes for each other.

0 of 5 carry a published Janka test.

WoodJankaDensity
Grandleaf seagrapeCoccoloba pubescens2,963 lbf*64.1 lb/ft³
SeagrapeCoccoloba uvifera2,064 lbf*54.2 lb/ft³
Swartz's pigeonplumCoccoloba swartzii1,725 lbf*49.9 lb/ft³
Tietongue, pigeon-plumCoccoloba diversifolia2,287 lbf*56.9 lb/ft³
UveraCoccoloba pyrifolia1,255 lbf*43.0 lb/ft³