Wood Record

genus

Copaifera

Woods sold under several trade names often come from one genus. These 5 share the genus Copaifera, so they are close relatives and frequent substitutes for each other.

4 of 5 carry a published Janka test.

WoodJankaDensity
CopaibaCopaifera officinalis1,475 lbf*46.4 lb/ft³
CopaíbaCopaifera sp.1,007 lbf37.5 lb/ft³
CopaíbaCopaifera multijuga1,067 lbf39.3 lb/ft³
CopaíbaCopaifera duckei1,464 lbf48.1 lb/ft³
CopaíbaCopaifera reticulata1,464 lbf48.1 lb/ft³