genus
Coprosma
Woods sold under several trade names often come from one genus. These 2 share the genus Coprosma, so they are close relatives and frequent substitutes for each other.
0 of 2 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Pubescent mirrorplantCoprosma pubens | 1,255 lbf* | 43.0 lb/ft³ |
| Woodland mirrorplantCoprosma rhynchocarpa | 1,475 lbf* | 46.4 lb/ft³ |