WoodJankaDensity
Anacahuita Texas OliveCordia boissieri1,203 lbf*42.1 lb/ft³
CanaleteCordia spp. (hard-wooded, dark-colored Gerascanthus group)2,200 lbf58.2 lb/ft³
Fragrant manjackCordia dichotoma451 lbf*26.7 lb/ft³
Frei-jorgeCordia sp.960 lbf*40.0 lb/ft³
FreijóCordia bicolor963 lbf37.1 lb/ft³
FreijóCordia goeldiana996 lbf36.3 lb/ft³
FreijóCordia sagotii882 lbf38.0 lb/ft³
KouCordia subcordata875 lbf*36.3 lb/ft³
Largeleaf geigertreeCordia sebestena1,309 lbf*43.8 lb/ft³
Laurel BlancoCordia spp. (soft-wooded, light-colored Alliodora group)1,000 lbf37.0 lb/ft³
Mucilage manjackCordia sulcata641 lbf*31.5 lb/ft³
MunecoCordia borinquensis1,788 lbf*50.7 lb/ft³
Red manjackCordia collococca915 lbf*37.1 lb/ft³
Spanish elmCordia alliodora915 lbf*37.1 lb/ft³
TouCordia aspera509 lbf*28.2 lb/ft³
West African CordiaCordia millenii590 lbf25.0 lb/ft³
ZiricoteCordia dodecandra2,530 lbf*59.6 lb/ft³