genus
Cornus
Woods sold under several trade names often come from one genus. These 4 share the genus Cornus, so they are close relatives and frequent substitutes for each other.
0 of 4 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Flowering dogwoodCornus florida | 1,725 lbf* | 49.9 lb/ft³ |
| Kousa dogwoodCornus kousa | 1,538 lbf* | 47.3 lb/ft³ |
| Pacific dogwoodCornus nuttallii | 1,363 lbf* | 44.7 lb/ft³ |
| Roughleaf dogwoodCornus drummondii | 1,538 lbf* | 47.3 lb/ft³ |