genus
Corymbia
Woods sold under several trade names often come from one genus. These 4 share the genus Corymbia, so they are close relatives and frequent substitutes for each other.
0 of 4 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Corymbia citriodoraCorymbia citriodora | 2,867 lbf* | 63.1 lb/ft³ |
| Red bloodwoodCorymbia gummifera | 2,139 lbf* | 55.1 lb/ft³ |
| RedgumCorymbia calophylla | 1,658 lbf* | 48.9 lb/ft³ |
| Spotted gumCorymbia maculata | 2,448 lbf* | 58.7 lb/ft³ |