Woods sold under several trade names often come from one genus. These 4 share the genus Couratari, so they are close relatives and frequent substitutes for each other.

3 of 4 carry a published Janka test.

WoodJankaDensity
MahotCouratari spp.960 lbf*37.0 lb/ft³
TauariCouratari oblongifolia936 lbf37.5 lb/ft³
TauariCouratari guianensis1,138 lbf39.6 lb/ft³
TauariCouratari stellata1,565 lbf50.7 lb/ft³