genus
Crataegus
Woods sold under several trade names often come from one genus. These 6 share the genus Crataegus, so they are close relatives and frequent substitutes for each other.
0 of 6 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Cockspur hawthornCrataegus crus-galli | 1,598 lbf* | 48.1 lb/ft³ |
| Downy hawthornCrataegus mollis | 1,852 lbf* | 51.5 lb/ft³ |
| Oneseed hawthornCrataegus monogyna | 1,725 lbf* | 49.9 lb/ft³ |
| Pear hawthornCrataegus calpodendron | 1,725 lbf* | 49.9 lb/ft³ |
| Scarlet hawthornCrataegus pedicellata | 1,788 lbf* | 50.7 lb/ft³ |
| Washington hawthornCrataegus phaenopyrum | 1,658 lbf* | 48.9 lb/ft³ |