Woods sold under several trade names often come from one genus. These 2 share the genus Crescentia, so they are close relatives and frequent substitutes for each other.

0 of 2 carry a published Janka test.

WoodJankaDensity
Common calabash treeCrescentia cujete1,103 lbf*40.5 lb/ft³
Houka, calabashCrescentia alata1,419 lbf*45.5 lb/ft³