2 of 10 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| African BlackwoodDalbergia melanoxylon | — | 83.0 lb/ft³ |
| Brazilian rosewoodDalbergia nigra | 2,720 lbf | 64.1 lb/ft³ |
| Brazilian tulipwoodDalbergia decipularis | 2,963 lbf* | 64.1 lb/ft³ |
| CocoboloDalbergia retusa | 3,860 lbf* | 69.0 lb/ft³ |
| CocoboloDalbergia tucurensis | 1,990 lbf* | 53.3 lb/ft³ |
| Honduras RosewoodDalbergia stevensonii | 3,097 lbf* | 63.0 lb/ft³ |
| Indian rosewoodDalbergia latifolia | 3,170 lbf | 53.0 lb/ft³ |
| Indian rosewoodDalbergia sissoo | 1,598 lbf* | 48.1 lb/ft³ |
| KingwoodDalbergia cearensis | 2,607 lbf* | 60.4 lb/ft³ |
| Siamese rosewoodDalbergia cochinchinensis | 3,441 lbf* | 68.7 lb/ft³ |