genus
Diospyros
Woods sold under several trade names often come from one genus. These 9 share the genus Diospyros, so they are close relatives and frequent substitutes for each other.
2 of 9 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| African ebonyDiospyros spp. | 3,220 lbf | 63.0 lb/ft³ |
| AuauliDiospyros samoensis | 1,725 lbf* | 49.9 lb/ft³ |
| Common persimmonDiospyros virginiana | 1,725 lbf* | 49.9 lb/ft³ |
| Diospyros ferreaDiospyros ferrea | 2,692 lbf* | 61.3 lb/ft³ |
| East Indian ebonyDiospyros spp. | 1,630 lbf | 52.0 lb/ft³ |
| LamaDiospyros sandwicensis | 2,607 lbf* | 60.4 lb/ft³ |
| MaboloDiospyros discolor | 3,147 lbf* | 65.9 lb/ft³ |
| PersimmonDiospyros kaki | 1,725 lbf* | 49.9 lb/ft³ |
| Texas persimmonDiospyros texana | 1,725 lbf* | 49.9 lb/ft³ |