Wood Record

genus

Entandrophragma

Woods sold under several trade names often come from one genus. These 4 share the genus Entandrophragma, so they are close relatives and frequent substitutes for each other.

3 of 4 carry a published Janka test.

WoodJankaDensity
Gedu NohorEntandrophragma angolense940 lbf34.0 lb/ft³
KosipoEntandrophragma candollei1,391 lbf*45.0 lb/ft³
SapeleEntandrophragma cylindricum1,510 lbf42.0 lb/ft³
UtileEntandrophragma utile1,260 lbf41.0 lb/ft³