Wood Record

genus

Erythrina

Woods sold under several trade names often come from one genus. These 7 share the genus Erythrina, so they are close relatives and frequent substitutes for each other.

0 of 7 carry a published Janka test.

WoodJankaDensity
BucayoErythrina fusca255 lbf*20.5 lb/ft³
Coral erythrinaErythrina corallodendron216 lbf*19.0 lb/ft³
CrybabytreeErythrina crista-galli255 lbf*20.5 lb/ft³
Gatae palagiErythrina subumbrans216 lbf*19.0 lb/ft³
Mountain immortelleErythrina poeppigiana321 lbf*22.8 lb/ft³
Tiger's clawErythrina variegata197 lbf*18.2 lb/ft³
Wili wiliErythrina sandwicensis276 lbf*21.2 lb/ft³