genus
Eschweilera
Woods sold under several trade names often come from one genus. These 4 share the genus Eschweilera, so they are close relatives and frequent substitutes for each other.
4 of 4 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| ManbarklakEschweilera spp. | 3,480 lbf | 46.2 lb/ft³ |
| MatamatáEschweilera coriacea | 2,467 lbf | 56.2 lb/ft³ |
| MatamatáEschweilera grandiflora = Eschweilera cf fracta | 1,995 lbf | 53.1 lb/ft³ |
| MatamatáEschweilera pedicellata = Eschweilera longipes | 2,410 lbf | 61.2 lb/ft³ |