genus
Eucalyptus
Woods sold under several trade names often come from one genus. These 29 share the genus Eucalyptus, so they are close relatives and frequent substitutes for each other.
4 of 29 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| AppleboxEucalyptus bridgesiana | 2,367 lbf* | 57.7 lb/ft³ |
| Argyle appleEucalyptus cinerea | 2,210 lbf* | 55.9 lb/ft³ |
| Australian tallowwoodEucalyptus microcorys | 3,054 lbf* | 65.0 lb/ft³ |
| Black ironboxEucalyptus raveretiana | 3,539 lbf* | 69.7 lb/ft³ |
| BlackbuttEucalyptus pilularis | 1,923 lbf* | 52.4 lb/ft³ |
| BluegumEucalyptus globulus | 2,060 lbf | 64.1 lb/ft³ |
| DegluptaEucalyptus deglupta | 470 lbf | 42.0 lb/ft³ |
| Forest redgumEucalyptus tereticornis | 2,367 lbf* | 57.7 lb/ft³ |
| Grand eucalyptusEucalyptus grandis | 1,309 lbf* | 43.8 lb/ft³ |
| Gray ironbarkEucalyptus paniculata | 3,647 lbf* | 70.6 lb/ft³ |
| JarrahEucalyptus marginata | 1,910 lbf | 54.0 lb/ft³ |
| KarriEucalyptus diversicolor | 2,040 lbf | 57.0 lb/ft³ |
| Manna gumEucalyptus viminalis | 1,923 lbf* | 52.4 lb/ft³ |
| Mountain graygumEucalyptus goniocalyx | 2,287 lbf* | 56.9 lb/ft³ |
| Narrowleaf red ironbarkEucalyptus crebra | 2,692 lbf* | 61.3 lb/ft³ |
| Red ironbarkEucalyptus sideroxylon | 3,147 lbf* | 65.9 lb/ft³ |
| RedboxEucalyptus polyanthemos | 2,867 lbf* | 63.1 lb/ft³ |
| RedmahoganyEucalyptus resinifera | 2,287 lbf* | 56.9 lb/ft³ |
| River red gumEucalyptus camaldulensis | 1,990 lbf* | 53.3 lb/ft³ |
| Roundleaf gumEucalyptus deanei | 1,852 lbf* | 51.5 lb/ft³ |
| Silver-dollar eucalyptusEucalyptus cordata | 1,054 lbf* | 39.6 lb/ft³ |
| Southern mahoganyEucalyptus botryoides | 2,064 lbf* | 54.2 lb/ft³ |
| SugargumEucalyptus cladocalyx | 2,867 lbf* | 63.1 lb/ft³ |
| SwampmahoganyEucalyptus robusta | 1,788 lbf* | 50.7 lb/ft³ |
| Sydney bluegumEucalyptus saligna | 1,419 lbf* | 45.5 lb/ft³ |
| TuartEucalyptus gomphocephala | 2,530 lbf* | 59.6 lb/ft³ |
| Western Australian floodedgumEucalyptus rudis | 1,475 lbf* | 46.4 lb/ft³ |
| White ironbarkEucalyptus leucoxylon | 2,692 lbf* | 61.3 lb/ft³ |
| YateEucalyptus cornuta | 3,147 lbf* | 65.9 lb/ft³ |