Wood Record

genus

Eugenia

Woods sold under several trade names often come from one genus. These 12 share the genus Eugenia, so they are close relatives and frequent substitutes for each other.

1 of 12 carry a published Janka test.

WoodJankaDensity
BirdcherryEugenia monticola2,779 lbf*62.2 lb/ft³
BlackrodwoodEugenia biflora1,990 lbf*53.3 lb/ft³
Christmas cherryEugenia pseudopsidium2,448 lbf*58.7 lb/ft³
KelatEugenia spp.1,198 lbf50.0 lb/ft³
LathberryEugenia cordata2,692 lbf*61.3 lb/ft³
Privet stopperEugenia ligustrina2,692 lbf*61.3 lb/ft³
Redberry stopperEugenia confusa3,241 lbf*66.9 lb/ft³
RockmyrtleEugenia procera2,692 lbf*61.3 lb/ft³
Serrette guaveEugenia domingensis1,788 lbf*50.7 lb/ft³
Stahl's stopperEugenia stahlii2,287 lbf*56.9 lb/ft³
Surinam cherryEugenia uniflora3,147 lbf*65.9 lb/ft³
White stopperEugenia axillaris2,064 lbf*54.2 lb/ft³