genus
Euphorbia
Woods sold under several trade names often come from one genus. These 3 share the genus Euphorbia, so they are close relatives and frequent substitutes for each other.
0 of 3 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Indian spurgetreeEuphorbia neriifolia | 451 lbf* | 26.7 lb/ft³ |
| Indiantree spurgeEuphorbia tirucalli | 542 lbf* | 29.1 lb/ft³ |
| PoinsettiaEuphorbia pulcherrima | 714 lbf* | 33.1 lb/ft³ |