genus
Ficus
Woods sold under several trade names often come from one genus. These 23 share the genus Ficus, so they are close relatives and frequent substitutes for each other.
1 of 23 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| AmateFicus obtusifolia | 608 lbf* | 30.7 lb/ft³ |
| AoaFicus obliqua | 791 lbf* | 34.7 lb/ft³ |
| AoaFicus prolixa | 423 lbf* | 26.0 lb/ft³ |
| Brown-woolly figFicus drupacea | 369 lbf* | 24.3 lb/ft³ |
| Chinese banyanFicus microcarpa | 1,103 lbf* | 40.5 lb/ft³ |
| Chinese banyanFicus thonningii | 791 lbf* | 34.7 lb/ft³ |
| Edible figFicus carica | 714 lbf* | 33.1 lb/ft³ |
| Ficus copiosaFicus copiosa | 915 lbf* | 37.1 lb/ft³ |
| Ficus luteaFicus lutea | 479 lbf* | 27.5 lb/ft³ |
| Figueira / gameleiraFicus insipida | 269 lbf | 28.1 lb/ft³ |
| Florida strangler figFicus aurea | 753 lbf* | 33.9 lb/ft³ |
| HigoFicus virens | 608 lbf* | 30.7 lb/ft³ |
| Indian banyanFicus benghalensis | 791 lbf* | 34.7 lb/ft³ |
| Indian rubberplantFicus elastica | 960 lbf* | 38.0 lb/ft³ |
| Jaguey blancoFicus trigonata | 714 lbf* | 33.1 lb/ft³ |
| Jamaican cherry figFicus americana | 608 lbf* | 30.7 lb/ft³ |
| MatiFicus tinctoria | 791 lbf* | 34.7 lb/ft³ |
| Peepul treeFicus religiosa | 679 lbf* | 32.3 lb/ft³ |
| Port Jackson figFicus rubiginosa | 679 lbf* | 32.3 lb/ft³ |
| Roxburgh figFicus auriculata | 714 lbf* | 33.1 lb/ft³ |
| Sycamore figFicus sycomorus | 791 lbf* | 34.7 lb/ft³ |
| Weeping figFicus benjamina | 915 lbf* | 37.1 lb/ft³ |
| Wild banyantree, shortleaf figFicus citrifolia | 832 lbf* | 35.5 lb/ft³ |