Woods sold under several trade names often come from one genus. These 15 share the genus Fraxinus, so they are close relatives and frequent substitutes for each other.

4 of 15 carry a published Janka test.

WoodJankaDensity
Berlandier ashFraxinus berlandieriana1,007 lbf*38.8 lb/ft³
Black ashFraxinus nigra850 lbf34.3 lb/ft³
Blue ashFraxinus quadrangulata1,107 lbf*40.6 lb/ft³
Carolina ashFraxinus caroliniana1,007 lbf*38.8 lb/ft³
Caucasian ashFraxinus oxycarpa1,203 lbf*42.1 lb/ft³
European ashFraxinus excelsior1,007 lbf*38.8 lb/ft³
Goodding's ashFraxinus gooddingii1,007 lbf*38.8 lb/ft³
Green ashFraxinus pennsylvanica1,200 lbf39.1 lb/ft³
Narrow-leafed ashFraxinus angustifolia1,007 lbf*38.8 lb/ft³
Oregon ashFraxinus latifolia1,160 lbf38.5 lb/ft³
Pumpkin ashFraxinus profunda875 lbf*36.3 lb/ft³
Shamel ashFraxinus uhdei1,203 lbf*42.1 lb/ft³
Texas ashFraxinus texensis1,007 lbf*38.8 lb/ft³
Velvet ashFraxinus velutina1,007 lbf*38.8 lb/ft³
White ashFraxinus americana1,320 lbf42.0 lb/ft³