genus
Garcinia
Woods sold under several trade names often come from one genus. These 6 share the genus Garcinia, so they are close relatives and frequent substitutes for each other.
0 of 6 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| GarciniaGarcinia myrtifolia | 2,367 lbf* | 57.7 lb/ft³ |
| Garcinia xanthochymusGarcinia xanthochymus | 2,530 lbf* | 59.6 lb/ft³ |
| GourkaGarcinia dulcis | 2,210 lbf* | 55.9 lb/ft³ |
| KandisGarcinia spp. | 2,530 lbf* | 58.0 lb/ft³ |
| MangosteenGarcinia mangostana | 2,530 lbf* | 59.6 lb/ft³ |
| Palo de cruzGarcinia portoricensis | 2,779 lbf* | 62.2 lb/ft³ |