Woods sold under several trade names often come from one genus. These 2 share the genus Gonystylus, so they are close relatives and frequent substitutes for each other.

2 of 2 carry a published Janka test.

WoodJankaDensity
principally G, bancanusGonystylus spp.1,300 lbf41.0 lb/ft³
RaminGonystylus bancanus1,300 lbf39.6 lb/ft³