Woods sold under several trade names often come from one genus. These 2 share the genus Grevillea, so they are close relatives and frequent substitutes for each other.

1 of 2 carry a published Janka test.

WoodJankaDensity
KahiliflowerGrevillea banksii1,255 lbf*43.0 lb/ft³
Silky-OakGrevillea robusta840 lbf38.0 lb/ft³