Wood Record

genus

Guapira

Woods sold under several trade names often come from one genus. These 2 share the genus Guapira, so they are close relatives and frequent substitutes for each other.

0 of 2 carry a published Janka test.

WoodJankaDensity
Black mampooGuapira fragrans960 lbf*38.0 lb/ft³
Corcho prietoGuapira obtusata1,054 lbf*39.6 lb/ft³