genus
Guarea
Woods sold under several trade names often come from one genus. These 4 share the genus Guarea, so they are close relatives and frequent substitutes for each other.
2 of 4 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| AlligatorwoodGuarea glabra | 1,309 lbf* | 43.8 lb/ft³ |
| American muskwoodGuarea guidonia | 1,363 lbf* | 44.7 lb/ft³ |
| CramanteeGuarea spp. | 1,065 lbf | 39.0 lb/ft³ |
| GuareaGuarea cedrata | 1,000 lbf | 36.0 lb/ft³ |