genus
Guatteria
Woods sold under several trade names often come from one genus. These 4 share the genus Guatteria, so they are close relatives and frequent substitutes for each other.
2 of 4 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Embira-pretaGuatteria olivacea | 883 lbf | 53.1 lb/ft³ |
| Embira-pretaGuatteria procera | 1,468 lbf | 50.7 lb/ft³ |
| Haya blancaGuatteria caribaea | 1,203 lbf* | 42.1 lb/ft³ |
| Haya mingaGuatteria blainii | 1,598 lbf* | 48.1 lb/ft³ |