Wood Record

genus

Guettarda

Woods sold under several trade names often come from one genus. These 5 share the genus Guettarda, so they are close relatives and frequent substitutes for each other.

0 of 5 carry a published Janka test.

WoodJankaDensity
Cucubano de monteGuettarda valenzuelana1,363 lbf*44.7 lb/ft³
Cucubano de viequesGuettarda odorata2,139 lbf*55.1 lb/ft³
Hammock velvetseedGuettarda elliptica2,064 lbf*54.2 lb/ft³
PuapuaGuettarda speciosa1,152 lbf*41.3 lb/ft³
Wild guaveGuettarda scabra1,852 lbf*51.5 lb/ft³