Wood Record

genus

Halesia

Woods sold under several trade names often come from one genus. These 4 share the genus Halesia, so they are close relatives and frequent substitutes for each other.

0 of 4 carry a published Janka test.

WoodJankaDensity
Carolina silverbellHalesia carolina641 lbf*31.5 lb/ft³
Little silverbellHalesia parviflora641 lbf*31.5 lb/ft³
Mountain silverbellHalesia tetraptera641 lbf*31.5 lb/ft³
Two-wing silverbellHalesia diptera641 lbf*31.5 lb/ft³