Woods sold under several trade names often come from one genus. These 2 share the genus Heritiera, so they are close relatives and frequent substitutes for each other.

1 of 2 carry a published Janka test.

WoodJankaDensity
MengkulangHeritiera spp.1,230 lbf42.0 lb/ft³
UfaHeritiera littoralis2,367 lbf*57.7 lb/ft³