genus
Hirtella
Woods sold under several trade names often come from one genus. These 2 share the genus Hirtella, so they are close relatives and frequent substitutes for each other.
0 of 2 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| PigeonberryHirtella triandra | 1,990 lbf* | 53.3 lb/ft³ |
| Teta de burra cinarronHirtella rugosa | 3,147 lbf* | 65.9 lb/ft³ |