Woods sold under several trade names often come from one genus. These 3 share the genus Homalium, so they are close relatives and frequent substitutes for each other.

2 of 3 carry a published Janka test.

WoodJankaDensity
African HomaliumHomalium spp.2,050 lbf54.0 lb/ft³
Burma LancewoodHomalium spp.2,270 lbf58.0 lb/ft³
White cogwoodHomalium racemosum2,210 lbf*55.9 lb/ft³