Woods sold under several trade names often come from one genus. These 6 share the genus Hymenolobium, so they are close relatives and frequent substitutes for each other.
6 of 6 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| AngelimHymenolobium sp | 1,422 lbf | 44.9 lb/ft³ |
| Angelim-pedraHymenolobium modestum | 1,647 lbf | 50.7 lb/ft³ |
| Angelim-pedraHymenolobium petraeum | 1,301 lbf | 44.3 lb/ft³ |
| Angelim-pedraHymenolobium pulcherrimum | 1,206 lbf | 44.3 lb/ft³ |
| Angelim-pedraHymenolobium nitidum | 1,257 lbf | 43.1 lb/ft³ |
| Para-angelimHymenolobium excelsum | 1,720 lbf | 47.0 lb/ft³ |