Wood Record

genus

Ilex

Woods sold under several trade names often come from one genus. These 9 share the genus Ilex, so they are close relatives and frequent substitutes for each other.

0 of 9 carry a published Janka test.

WoodJankaDensity
American hollyIlex opaca960 lbf*38.0 lb/ft³
CatberryIlex mucronata960 lbf*38.0 lb/ft³
DahoonIlex cassine1,152 lbf*41.3 lb/ft³
English hollyIlex aquifolium1,852 lbf*51.5 lb/ft³
GongolinIlex sideroxyloides1,788 lbf*50.7 lb/ft³
Hawaii hollyIlex anomala791 lbf*34.7 lb/ft³
MateIlex paraguariensis960 lbf*38.0 lb/ft³
Puerto Rico hollyIlex nitida2,139 lbf*55.1 lb/ft³
YauponIlex vomitoria1,054 lbf*39.6 lb/ft³