WoodJankaDensity
Ice cream beanInga edulis1,054 lbf*39.6 lb/ft³
IngáInga paraensis3,064 lbf65.9 lb/ft³
IngáInga sp2,846 lbf68.7 lb/ft³
Ingá / ingá xixiInga alba1,418 lbf48.1 lb/ft³
Inga nobilisInga nobilis1,363 lbf*44.7 lb/ft³
River kokoInga vera1,007 lbf*38.8 lb/ft³
Sacky sac beanInga laurina1,788 lbf*50.7 lb/ft³