Woods sold under several trade names often come from one genus. These 8 share the genus Juglans, so they are close relatives and frequent substitutes for each other.
2 of 8 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Arizona walnutJuglans major | 714 lbf* | 33.1 lb/ft³ |
| Black walnutJuglans nigra | 1,010 lbf | 38.5 lb/ft³ |
| ButternutJuglans cinerea | 490 lbf | 26.6 lb/ft³ |
| English walnutJuglans regia | 714 lbf* | 33.1 lb/ft³ |
| NogalJuglans spp. | 960 lbf* | 38.0 lb/ft³ |
| Northern California black walnutJuglans hindsii | 714 lbf* | 33.1 lb/ft³ |
| Southern California black walnutJuglans californica | 714 lbf* | 33.1 lb/ft³ |
| Texas walnutJuglans microcarpa | 714 lbf* | 33.1 lb/ft³ |