Wood Record

genus

Juniperus

Woods sold under several trade names often come from one genus. These 14 share the genus Juniperus, so they are close relatives and frequent substitutes for each other.

0 of 14 carry a published Janka test.

WoodJankaDensity
African Pencil CedarJuniperus procera717 lbf*36.0 lb/ft³
Alligator juniperJuniperus deppeana717 lbf*36.3 lb/ft³
Ashe juniperJuniperus ashei645 lbf*33.9 lb/ft³
Bermuda juniperJuniperus bermudiana792 lbf*38.8 lb/ft³
California juniperJuniperus californica645 lbf*33.9 lb/ft³
Chinese juniperJuniperus chinensis645 lbf*33.9 lb/ft³
Drooping juniperJuniperus flaccida645 lbf*33.9 lb/ft³
Eastern redcedarJuniperus virginiana615 lbf*32.8 lb/ft³
Oneseed juniperJuniperus monosperma645 lbf*33.9 lb/ft³
Pinchot juniperJuniperus pinchotii645 lbf*33.9 lb/ft³
Redberry juniperJuniperus coahuilensis645 lbf*33.9 lb/ft³
Rocky Mountain juniperJuniperus scopulorum645 lbf*33.9 lb/ft³
Utah juniperJuniperus osteosperma1,282 lbf*53.3 lb/ft³
Western juniperJuniperus occidentalis645 lbf*33.9 lb/ft³