Woods sold under several trade names often come from one genus. These 4 share the genus Larix, so they are close relatives and frequent substitutes for each other.

2 of 4 carry a published Janka test.

WoodJankaDensity
European larchLarix decidua740 lbf*37.1 lb/ft³
Subalpine larchLarix lyallii740 lbf*37.1 lb/ft³
TamarackLarix laricina590 lbf37.1 lb/ft³
Western larchLarix occidentalis830 lbf36.3 lb/ft³