genus
Licaria
Woods sold under several trade names often come from one genus. These 4 share the genus Licaria, so they are close relatives and frequent substitutes for each other.
2 of 4 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| KaneelhartLicaria spp. | 2,900 lbf | 62.0 lb/ft³ |
| Louro-amareloLicaria chrysophylla = Licaria rigida | 2,019 lbf | 57.7 lb/ft³ |
| Pepperleaf sweetwoodLicaria triandra | 1,923 lbf* | 52.4 lb/ft³ |
| Puerto Rico cinnamonLicaria parvifolia | 2,367 lbf* | 57.7 lb/ft³ |