genus
Ligustrum
Woods sold under several trade names often come from one genus. These 4 share the genus Ligustrum, so they are close relatives and frequent substitutes for each other.
0 of 4 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| California privetLigustrum ovalifolium | 1,300 lbf* | 43.7 lb/ft³ |
| Chinese privetLigustrum sinense | 1,852 lbf* | 51.5 lb/ft³ |
| Glossy privetLigustrum lucidum | 1,203 lbf* | 42.1 lb/ft³ |
| Japanese privetLigustrum japonicum | 1,203 lbf* | 42.1 lb/ft³ |