Woods sold under several trade names often come from one genus. These 2 share the genus Macadamia, so they are close relatives and frequent substitutes for each other.
0 of 2 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Macadamia NutMacadamia tetraphylla | 1,538 lbf* | 47.3 lb/ft³ |
| Macadamia nut tree, penguaMacadamia integrifolia | 2,064 lbf* | 54.2 lb/ft³ |