Woods sold under several trade names often come from one genus. These 2 share the genus Macaranga, so they are close relatives and frequent substitutes for each other.

0 of 2 carry a published Janka test.

WoodJankaDensity
Parasol leaf treeMacaranga tanarius479 lbf*27.5 lb/ft³
PenguaMacaranga mappa423 lbf*26.0 lb/ft³