Woods sold under several trade names often come from one genus. These 12 share the genus Magnolia, so they are close relatives and frequent substitutes for each other.

3 of 12 carry a published Janka test.

WoodJankaDensity
Bigleaf magnoliaMagnolia macrophylla679 lbf*32.3 lb/ft³
CucumbertreeMagnolia acuminata700 lbf33.6 lb/ft³
Fraser magnoliaMagnolia fraseri573 lbf*29.8 lb/ft³
Laurel magnoliaMagnolia splendens1,203 lbf*42.1 lb/ft³
MagnoliaMagnolia spp.1,090 lbf39.0 lb/ft³
Oyama magnoliaMagnolia sieboldii679 lbf*32.3 lb/ft³
Puerto Rico magnoliaMagnolia portoricensis1,203 lbf*42.1 lb/ft³
Pyramid magnoliaMagnolia pyramidata679 lbf*32.3 lb/ft³
Southern magnoliaMagnolia grandiflora1,020 lbf35.0 lb/ft³
Star magnoliaMagnolia stellata679 lbf*32.3 lb/ft³
Sweetbay magnoliaMagnolia virginiana875 lbf*36.3 lb/ft³
Umbrella magnoliaMagnolia tripetala679 lbf*32.3 lb/ft³