genus
Malus
Woods sold under several trade names often come from one genus. These 8 share the genus Malus, so they are close relatives and frequent substitutes for each other.
0 of 8 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| AppleMalus domestica | 1,658 lbf* | 48.9 lb/ft³ |
| Japanese flowering crab appleMalus floribunda | 1,538 lbf* | 47.3 lb/ft³ |
| Oregon crab appleMalus fusca | 1,538 lbf* | 47.3 lb/ft³ |
| Paradise appleMalus pumila | 1,538 lbf* | 47.3 lb/ft³ |
| Prairie crab appleMalus ioensis | 1,538 lbf* | 47.3 lb/ft³ |
| Siberian crab appleMalus baccata | 1,538 lbf* | 47.3 lb/ft³ |
| Southern crab appleMalus angustifolia | 1,538 lbf* | 47.3 lb/ft³ |
| Sweet crab appleMalus coronaria | 1,538 lbf* | 47.3 lb/ft³ |