Mangifera

Woods sold under several trade names often come from one genus. These 4 share the genus Mangifera, so they are close relatives and frequent substitutes for each other.

1 of 4 carry a published Janka test.

WoodJankaDensity
KanitMangifera minor1,255 lbf*43.0 lb/ft³
MangoMangifera spp.1,000 lbf40.0 lb/ft³
MangoMangifera indica1,103 lbf*40.5 lb/ft³
Saipan mangoMangifera odorata1,054 lbf*39.6 lb/ft³