genus
Manilkara
Woods sold under several trade names often come from one genus. These 6 share the genus Manilkara, so they are close relatives and frequent substitutes for each other.
3 of 6 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| BulletwoodManilkara bidentata | 3,190 lbf | 66.0 lb/ft³ |
| MaçarandubaManilkara sp. | 3,228 lbf | 66.8 lb/ft³ |
| MaçarandubaManilkara huberi | 3,047 lbf | 66.8 lb/ft³ |
| PaniManilkara dissecta | 3,749 lbf* | 71.5 lb/ft³ |
| SapodillaManilkara zapota | 3,054 lbf* | 65.0 lb/ft³ |
| Wild dillyManilkara jaimiqui | 3,147 lbf* | 65.9 lb/ft³ |