genus
Maytenus
Woods sold under several trade names often come from one genus. These 2 share the genus Maytenus, so they are close relatives and frequent substitutes for each other.
1 of 2 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Carne D'AntaMaytenus spp. | 2,240 lbf | 54.0 lb/ft³ |
| MaytenMaytenus boaria | 1,538 lbf* | 47.3 lb/ft³ |