Woods sold under several trade names often come from one genus. These 2 share the genus Melaleuca, so they are close relatives and frequent substitutes for each other.

0 of 2 carry a published Janka test.

WoodJankaDensity
Broad-Leaved Tea-TreeMelaleuca quinquenervia1,788 lbf*50.0 lb/ft³
Cajeput treeMelaleuca linariifolia1,054 lbf*39.6 lb/ft³