genus
Melochia
Woods sold under several trade names often come from one genus. These 2 share the genus Melochia, so they are close relatives and frequent substitutes for each other.
0 of 2 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Hierba del soldadoMelochia umbellata | 451 lbf* | 26.7 lb/ft³ |
| TeabushMelochia tomentosa | 2,064 lbf* | 54.2 lb/ft³ |