Wood Record

genus

Metrosideros

Woods sold under several trade names often come from one genus. These 2 share the genus Metrosideros, so they are close relatives and frequent substitutes for each other.

1 of 2 carry a published Janka test.

WoodJankaDensity
OhiaMetrosideros collina subsp. polymorpha2,090 lbf57.0 lb/ft³
Ohia lehuaMetrosideros polymorpha1,923 lbf*52.4 lb/ft³