| Wood | Janka | Density |
|---|---|---|
| AuqueyMiconia punctata | 1,419 lbf* | 45.5 lb/ft³ |
| Camasey cuatrocanalesMiconia mirabilis | 1,203 lbf* | 42.1 lb/ft³ |
| Camasey de costillaMiconia impetiolaris | 1,598 lbf* | 48.1 lb/ft³ |
| Camasey felpaMiconia racemosa | 1,054 lbf* | 39.6 lb/ft³ |
| Granadillo boboMiconia prasina | 1,363 lbf* | 44.7 lb/ft³ |
| Jau jauMiconia serrulata | 1,309 lbf* | 43.8 lb/ft³ |
| RajadorMiconia tetrandra | 1,852 lbf* | 51.5 lb/ft³ |
| SaquiyacMiconia affinis | 1,475 lbf* | 46.4 lb/ft³ |
| Velvet treeMiconia calvescens | 1,103 lbf* | 40.5 lb/ft³ |